Processing Properties Metric English Comments
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with ..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low ..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications. Torlon PAI has the highest..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
Torlon® 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a ..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not ..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)
Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber
Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber
Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal..
Back Pressure 6.89 - 27.6 MPa
1000 - 4000 psi
Denka STYROL MW1 Polystyrene
"DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," ..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)  (discontinued **)
Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P..
Back Pressure 6.89 MPa
999 psi
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp..