Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.345 - 2.07 MPa | 50.0 - 300 psi | |
Clariant ABS4500 ABS, High Impact Data provided by Clariant Masterbatches |
|||
Back Pressure | 0.345 - 2.07 MPa | 50.0 - 300 psi | |
Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy Data provided by Clariant Masterbatches |