Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 51.7 - 65.6 °C | 125 - 150 °F | |
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 51.7 - 65.6 °C | 125 - 150 °F | |
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 51.7 - 65.6 °C | 125 - 150 °F | |
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 51.7 - 65.6 °C | 125 - 150 °F | |
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 51.7 - 65.6 °C | 125 - 150 °F | |
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 51.7 - 65.6 °C | 125 - 150 °F | |
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 51.7 - 54.4 °C | 125 - 130 °F | |
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish.. |
|||
Drying Temperature | 51.7 - 54.4 °C | 125 - 130 °F | |
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi.. |
|||
Drying Temperature | 51.7 - 54.4 °C | 125 - 130 °F | |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Drying Temperature | 51.7 °C @Time 7200 - 14400 sec |
125 °F @Time 2.00 - 4.00 hour |
|
RTP Company RTP 6001-40A Specialty Thermoplastic Elastomer |
|||
Drying Temperature | 51.7 °C @Time 7200 - 14400 sec |
125 °F @Time 2.00 - 4.00 hour |
|
RTP Company RTP 6001-70A Specialty Thermoplastic Elastomer |
|||
Drying Temperature | 51.7 °C | 125 °F | |
RTP Company RTP 6035-45A Specialty Thermoplastic Elastomer, Clear |
|||
Drying Temperature | 51.7 - 100 °C | 125 - 212 °F | Average value: 75.3 °C Grade Count:137 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® D 4107 C Black TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good I.. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R.. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 3540 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 7025 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 7321 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantUV Resistance, Good Processability, Good.. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 7455 ER TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 7727 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 8030 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 9002 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® D 3604 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Drying Temperature | 51.7 °C @Time 7200 - 14400 sec |
125 °F @Time 2.00 - 4.00 hour |
|
RTP Company RTP 2740 S-70A Saturated Styrenic Block Copolymer, General Purpose |
|||
Drying Temperature | 51.7 °C @Time 7200 - 14400 sec |
125 °F @Time 2.00 - 4.00 hour |
|
RTP Company RTP 6001-50A Specialty Thermoplastic Elastomer |
|||
Drying Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 6202 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Drying Temperature | 51.7 °C @Time 7200 - 21600 sec |
125 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 115375 C Bio-Based Polylactic Acid (PLA), PLA-PMMA Alloy - Transparent - 39% Renewable Resource Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |