Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 70.0 - 71.0 °C | 158 - 160 °F | Average value: 70.1 °C Grade Count:11 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Drying Temperature | 60.0 - 71.1 °C | 140 - 160 °F | |
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated
&nb Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 60.0 - 71.1 °C | 140 - 160 °F | |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 54.4 - 71.1 °C | 130 - 160 °F | |
PolyOne Edgetek® AS-20GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 60.0 - 71.0 °C | 140 - 160 °F | |
PolyOne Lubri-Tech™ AS-000/10T-2S ABS - 10% PTFE - 2% Silicone
(discontinued **) Data provided by PolyOne. |