Processing Properties Metric English Comments
Drying Temperature 50.0 °C

@Time 14400 sec
122 °F

@Time 4.00 hour
NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware
NatureWorks® PLA polymer AW 240D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed ..
Drying Temperature 50.0 - 55.0 °C

@Time >=10800 sec
122 - 131 °F

@Time >=3.00 hour
If stored for longer than 1 year
Premix Thermoplastics PRE-ELEC® CP 1318  (discontinued **)
PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit..
Drying Temperature 50.0 - 149 °C
122 - 300 °F
Average value: 99.4 °C Grade Count:33
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Drying Temperature 50.0 - 140 °C
122 - 284 °F
Average value: 96.1 °C Grade Count:24
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
Drying Temperature 50.0 - 150 °C
122 - 302 °F
Average value: 130 °C Grade Count:14
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max..
Drying Temperature 50.0 - 150 °C
122 - 302 °F
Average value: 122 °C Grade Count:15
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu..
Drying Temperature 50.0 - 60.0 °C
122 - 140 °F
Kostat BK-STAT
BK-STAT is an inherently dissipative polymer incorporated into a variety of resins as a melt additive. The electrical resistivity is reduced by formation of a conductive percolating network in the ..
Drying Temperature 50.0 °C
122 °F
Borealis Supersmooth™ LE0500 Crosslinkable Semiconductive Shielding Compound
Supersmooth LE0500 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0500 is based on an ethylene butyl acry..
Drying Temperature 50.0 °C
122 °F
Eastman Eastar CN005 Copolyester, High Flow Grade
Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit..
Drying Temperature 50.0 °C
122 °F
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release
Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit..
Drying Temperature 50.0 - 140 °C
122 - 284 °F
Average value: 102 °C Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..