NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polylactic Acid (PLA) Biopolymer
Manufacturer NatureWorks LLC
Trade Name Ingeo™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NatureWorks® PLA polymer AW 240D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed for use in food service ware applications. Ingeo AW 240D is an opaque, off-white extrusion grade that is fully formulated to be used naturally, but may be blended with color compounds. Extruded roll stock is thermoformable.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 210 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
Mechanical Properties Metric English Comments
Flexural Modulus 1.65 GPa
239 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Processing Properties Metric English Comments
Feed Temperature 170 °C
338 °F
Adapter Temperature 185 °C
365 °F
Die Temperature 185 °C
365 °F
Melt Temperature 185 °C
365 °F
Drying Temperature 50.0 °C

@Time 14400 sec
122 °F

@Time 4.00 hour
Moisture Content <= 0.025 %
<= 0.025 %
Dew Point -40.0 °C
-40.0 °F
Drying Air Flow Rate >= 14.2 l/min
>= 0.500 ft³/min (CFM)
Screw Speed 20 - 100 rpm
20 - 100 rpm