Polymer Property : Rear Barrel Temperature = 580 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 293 - 304 °C
560 - 580 °F
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified
Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Rear Barrel Temperature 293 - 304 °C
560 - 580 °F
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized
Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
Rear Barrel Temperature 293 - 304 °C
560 - 580 °F
Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced
Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced
Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro..
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP5 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP6 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP7 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Rear Barrel Temperature 282 - 304 °C
540 - 580 °F
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Rear Barrel Temperature 288 - 304 °C
550 - 580 °F
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 288 - 304 °C
550 - 580 °F
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 293 - 304 °C
560 - 580 °F
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 288 - 304 °C
550 - 580 °F
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 288 - 304 °C
550 - 580 °F
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 282 - 304 °C
540 - 580 °F
Wellman EcoLon® 2000-BK1 37% Post Consumer Compound Nylon 66
Description: Post Consumer Compound Nylon 66Information provided by Wellman.
Rear Barrel Temperature 282 - 304 °C
540 - 580 °F
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
Rear Barrel Temperature 282 - 304 °C
540 - 580 °F
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
Rear Barrel Temperature 282 - 304 °C
540 - 580 °F
Wellman Wellamid® GS40-66 22L-N 40% Glass Sphere Filled Nylon 66, Lubricated
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
Rear Barrel Temperature 282 - 304 °C
540 - 580 °F
Wellman Wellamid® GSF25/15-66 22L-N 40% Glass Sphere/Fiber Reinforced Nylon 66
Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman.
Rear Barrel Temperature 282 - 304 °C
540 - 580 °F
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Rear Barrel Temperature 282 - 304 °C
540 - 580 °F
Wellman Wellamid® MRT1487-N Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.