Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 243 °C | 470 °F | |
Oxford Polymers PBT 30GF PBT, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and LubricantsSpecial Characteris.. |
|||
Rear Barrel Temperature | 243 - 293 °C | 470 - 560 °F | |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Rear Barrel Temperature | 243 - 293 °C | 470 - 560 °F | |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Rear Barrel Temperature | 243 - 293 °C | 470 - 560 °F | |
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Rear Barrel Temperature | 243 - 293 °C | 470 - 560 °F | |
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Rear Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test.. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hybrid B3030U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Rear Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
Polymer Resources TP-M30 Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate Information provided by Ravago. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate Information provided by Ravago. |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
LTL Color Compounds ColorFast® FRPBT130 PBT, 30% Glass-Filled 30% glass-filled V-0 rated PBT - UL listedAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded 13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 243 - 271 °C | 470 - 520 °F | |
Star Plastics PC/PBT7820 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 243 - 271 °C | 470 - 520 °F | |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 243 - 271 °C | 470 - 520 °F | |
Star Plastics PC/PET7901 Molding Grade PC/PET Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Samyang Trirex® PC-3020U 22 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Entec Hylex® P1017FR Polycarbonate Information provided by Ravago. |
|||
Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 243 - 293 °C | 470 - 560 °F | |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |