Polymer Property : Nozzle Temperature = 437 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 215 - 225 °C
419 - 437 °F
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane
Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica..
Nozzle Temperature 200 - 225 °C
392 - 437 °F
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene
Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc..
Nozzle Temperature 210 - 225 °C
410 - 437 °F
Injection
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester
Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN ..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ P75A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P90A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 215 - 225 °C
419 - 437 °F
Injection
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 215 - 225 °C
419 - 437 °F
Injection
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer
Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 215 - 225 °C
419 - 437 °F
Injection
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer
Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 215 - 225 °C
419 - 437 °F
Injection
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer
Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 195 - 225 °C
383 - 437 °F
Injection
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..