Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 215 °C | 419 °F | Nozzle (Melt) |
ExxonMobil Escorene® HD-6705 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, Good Stiffness, Good ImpactUses: Food containers, Housewares, Toys |
|||
Nozzle Temperature | 215 - 235 °C | 419 - 455 °F | Injection Molding |
LG Chemical KEYFLEX BT 1245D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Medium Modulus, Black colorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Lubrizol Advanced Materials Pearlthane® D91T86 Thermoplastic Polyurethane Type : Pearlthane® D91T86 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
Nozzle Temperature | 215 - 225 °C | 419 - 437 °F | |
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica.. |
|||
Nozzle Temperature | 215 °C | 419 °F | |
SK Chemicals SKYTHANE® S160D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Nozzle Temperature | 215 °C | 419 °F | |
SK Chemicals SKYTHANE® S168D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Nozzle Temperature | 215 °C | 419 °F | |
SK Chemicals SKYTHANE® S360D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Nozzle Temperature | 215 °C | 419 °F | |
SK Chemicals SKYTHANE® S368D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Nozzle Temperature | 215 - 230 °C | 419 - 446 °F | |
Lubrizol Estane® S160D Thermoplastic Polyurethane Type: Estane® S160D is a Shore 63D, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Nozzle Temperature | 215 - 230 °C | 419 - 446 °F | |
Lubrizol Estane® S360D Thermoplastic Polyurethane Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Nozzle Temperature | 215 - 230 °C | 419 - 446 °F | |
Lubrizol Estane® S364D Thermoplastic Polyurethane Type: Estane® S364D is a Shore 65D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Nozzle Temperature | 215 °C | 419 °F | Injection |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Nozzle Temperature | 215 °C | 419 °F | Injection |
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Nozzle Temperature | 215 - 225 °C | 419 - 437 °F | Injection |
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 215 - 225 °C | 419 - 437 °F | Injection |
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 215 - 225 °C | 419 - 437 °F | Injection |
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 215 - 225 °C | 419 - 437 °F | Injection |
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL1100 ABS General Purpose Grade High gloss, excellent external appearanceInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL1200 ABS General Purpose Grade Middle impact, Good mechanical strength, High flexural strengthInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL2100 ABS Good Flow Grade Good flow, Easy processing, High glossInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL3200 ABS Flame-Retardant Grade Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL3300 ABS Flame-Retardant Grade Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL5200 ABS Extrusion Grade Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL6000 ABS Metal Plating Grade Excellent plating performance, Good thermal stabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL1300 ABS General Purpose Grade Excellent impact properties at low temperaturesInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL3100 ABS Flame-Retardant Grade Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Beijing Chemical Industry KAIFA® GL5100 ABS Extrusion Grade Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 215 °C | 419 °F | |
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |