Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
Green Dot Terratek® BD 4015 Biodegradable Polymer Terratek BD biodegradable composites are created from a proprietary blend of starch-based ingredients and other materials, the natural components derived from renewable grain sources account for the.. |
|||
Front Barrel Temperature | 166 - 182 °C | 330 - 360 °F | |
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit.. |
|||
Front Barrel Temperature | 166 - 182 °C | 330 - 360 °F | |
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and .. |
|||
Front Barrel Temperature | 166 - 182 °C | 330 - 360 °F | |
Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer Elastocon® 2855 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2855 is FDA compliant and well suited for cons.. |
|||
Front Barrel Temperature | 160 - 182 °C | 320 - 360 °F | |
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited.. |
|||
Front Barrel Temperature | 177 - 182 °C | 350 - 360 °F | |
Elastocon TPE Technologies Elastocon® 8068B Thermoplastic Elastomer Elastocon® 8068B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068B is well suited for consumer goods an.. |
|||
Front Barrel Temperature | 177 - 182 °C | 350 - 360 °F | |
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui.. |
|||
Front Barrel Temperature | 177 - 182 °C | 350 - 360 °F | |
Elastocon TPE Technologies Elastocon® 8068L Thermoplastic Elastomer Elastocon® 8068L is a colorable lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068L is well .. |
|||
Front Barrel Temperature | 177 - 182 °C | 350 - 360 °F | |
Elastocon TPE Technologies Elastocon® 8068N Thermoplastic Elastomer Elastocon® 8068N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068N is FDA compliant and well suited.. |
|||
Front Barrel Temperature | 160 - 182 °C | 320 - 360 °F | |
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer.. |