Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastocon® 2855 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2855 is FDA compliant and well suited for consumer products and medical applications. Elastocon® 2855 can be overmolded onto polypropylene.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
ASTM D792
Linear Mold Shrinkage 0.016 - 0.026 cm/cm
0.016 - 0.026 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
ASTM D2240
Tensile Strength, Yield 6.55 MPa
950 psi
ASTM D412
Elongation at Break 660 %
660 %
ASTM D412
100% Modulus 0.00212 GPa
0.308 ksi
ASTM D412
Compression Set 25 %

@Time 79200 sec
25 %

@Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Rear Barrel Temperature 149 - 166 °C
300 - 330 °F
Front Barrel Temperature 166 - 182 °C
330 - 360 °F
Nozzle Temperature 188 - 216 °C
370 - 420 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.689 - 1.38 MPa
100 - 200 psi