Nabaltec GRANALOX® NM 9916 F Ceramic Body

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Nabaltec GmbH
Trade Name GRANALOX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec GRANALOX® NM 9916 F Ceramic Body.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum are tailored to the application areas in which the material is used such as wear resistance, high temperature stability, good electrical insulation, thermal conductivity and corrosion resistance.Used in engineering ceramics.Information provided by Nabaltec.
Physical Properties Metric English Comments
Bulk Density 1.10 - 1.20 g/cc
0.0397 - 0.0434 lb/in³
Density 3.88 - 3.92 g/cc
0.140 - 0.142 lb/in³
Sintered
Moisture Absorption at Equilibrium 0.30 - 0.50 %
0.30 - 0.50 %
Loss On Ignition 5.0 %
5.0 %
Particle Size 80 - 120 µm
80 - 120 µm
Mean Granulate Size
Thermal Properties Metric English Comments
Shrinkage 17 - 18 %
17 - 18 %
linear
Component Elements Properties Metric English Comments
Al2O3 99.6 %
99.6 %
Na2O 0.10 %
0.10 %
Processing Properties Metric English Comments
Sintering Temperature 1600 - 1700 °C
2910 - 3090 °F
Interval (dense ceramic parts)
1620 °C

@Time 7200 sec
2950 °F

@Time 2.00 hour