Processing Properties Metric English Comments
Hold Pressure 60.0 - 100 MPa
8700 - 14500 psi
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade
Information provided by Eurotec®
Hold Pressure 60.0 - 100 MPa
8700 - 14500 psi
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black
Information provided by Eurotec®
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey
Information provided by Eurotec®