Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Celanese Celanex® 2300 GV3/30 PBT, 30% Glass Reinforced
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: PBT30% Glass bead reinforced gradeInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Celanese Celanex® 2500 PBT
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: PBTBasic gradeInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Celcon® UV25Z POM, UV Resistant
(Unverified Data**) Celcon® UV25Z is a nominal 2.5 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposur.. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 13021 POM
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with moderate flowInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 2521 LS POM, UV Resistant
(Unverified Data**) Stiff-flowing grade for injection molding and extrusion, UV resistantInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 M POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with molybdenum disulphide modifiedInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 XAP² ™ POM
(Unverified Data**) POM copolymerLow EmissionInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® MT8F01 POM, Medical Technology
(Unverified Data**) Hostaform® acetal copolymer grade MT8F01 is a special grade developed for medical industry applications containing low residual monomers. Hostaform® MT8F01 is a standard flow low level polytetrafl.. |
|||
Hold Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Eurotec® Tecopet® PT74 CR30 BK111 PR PET, 30% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Eurotec® Tecotek® PC44 GR10 GR003 ZG70 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), light grey Information provided by Eurotec® |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Celcon® M90UV POM, UV Resistant Celcon« M90UV is an acetal copolymer developed as a natural UV light stabilized standard flow grade for overall performance in most molding applications. It has been formulated as a natural acetal .. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Celcon® WR90Z POM, UV Resistant Celcon« WR90Z is a standard nominal 9 melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications while retaining a good balance of .. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Celstran® POM-GF25-04 AF3001 POM, 25% Glass Reinforced Material code according to ISO 1043-1: POMInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® AM90S POM, Specialty Hostaform« acetal copolymer grade AM90S is a standard melt flow acetal copolymer grade containing an antimicrobial ingredient. Hostaform« AM90S provides the same physical and mechanical performan.. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 G POM, Tribological Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® TF-10XAP® POM, Impact Modified Hostaform« acetal copolymer TF-10 XAP« is low emission, improved flow, impact modified grade providing optimum performance in general purpose injection molding primarily for the interior automot.. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® XGC25 POM, 25% Glass Reinforced Hostaform« XGC25 is a Polyacetalcopolymer reinforced with approx. 25% glass fibres. Compared to the Hostaform« C 9021 GV 1/30 Hostaform« XGC25 has a higher strength.Information provided by Cel.. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 13021 POM, Unfilled Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 13031 POM, Unfilled Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 XAP² ™ POM, Unfilled POM copolymerInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® EC140CF10 POM, 10% Specialty Hostaform« acetal copolymer grade EC140CF10 is a 10% carbon fiber reinforced grade for increase strength, stiffness and electrical conductivity.Information provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 M XAP2® POM Description: Injection molding type, modified with molybdenum disulphide; good chemical resistance to solvents, fuel and strong alkalis as well as good hydrolysis resistance; high resistance to ther.. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 TF XAP² POM, Tribological Chemical abbreviation according to ISO 1043-1: POMIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorre.. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® S 9243 XAP2 ™ POM, Impact Modified POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi.. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 13031 XF POM, Specialty
(Unverified Data**) Hostaform® acetal copolymer grade C13031 XF is an acetal copolymer modified to resist deterioration from aggressive fuel blends. This material is specially targeted for transportation industry fu.. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 SW POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, special modified with anti-friction additives for prevention of squeaking noiseInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® EC140CF10 POM, 10% Specialty
(Unverified Data**) Hostaform® acetal copolymer grade EC140CF10 is a 10% carbon fiber reinforced grade for increase strength, stiffness and electrical conductivity.10% carbon fiber, electrostatic dissipative gradeInfo.. |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® S 9243 XAP² ™ POM, Impact Modified
(Unverified Data**) POM copolymer, modifiedImpact modified, low emissionInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 GV1/20 POM, 20% Glass Reinforced Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 GV3/10 POM, 10% Glass Reinforced Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |