Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural
Information provided by Eurotec®
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Eurotec® Tecotek® PC44 GR10 GR003 ZG70 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), light grey
Information provided by Eurotec®