Processing Properties Metric English Comments
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® M270UV POM, UV Resistant  (Unverified Data**)
Celcon® M270UV is an acetal copolymer developed as a natural UV light stabilized lower molecular weight, high-flow grade designed for superior moldability in multi-cavity or hard to fill injection ..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® M90™ POM  (Unverified Data**)
Celcon acetal copolymer grade M90™ is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film. This gr..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® MC90-HM POM, Mineral Reinforced  (Unverified Data**)
Celcon® MC90-HM is a highly mineral filled and coupled M90 material for producing very flat and dimensionally stable parts (normal flow).Mineral coupled for reduced warpage, high modulus, moderate ..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® UV25Z POM, UV Resistant  (Unverified Data**)
Celcon® UV25Z is a nominal 2.5 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposur..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 13031 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with moderate flow, about 10% higher strength, rigidity and hardness than C 13021Information provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 9021 SW XAP² ™ LS POM, Tribological  (Unverified Data**)
POM copolymerTribological, Low EmissionInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 9021 XAP² ™ POM  (Unverified Data**)
POM copolymerLow EmissionInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® EC140XF POM, Specialty  (Unverified Data**)
Hostaform® EC140XF is a conductive ESD grade of acetal copolymer for applications requiring dissipation of static build-up. EC140XF has an improved resistance to aggressive fuel blends.electrosta..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® MT8F01 POM, Medical Technology  (Unverified Data**)
Hostaform® acetal copolymer grade MT8F01 is a special grade developed for medical industry applications containing low residual monomers. Hostaform® MT8F01 is a standard flow low level polytetrafl..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Eurotec® Tecotek® PC30 NL RX PC, unfilled, improved flow & low temperature impact, natural
Information provided by Eurotec®
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® M90SW POM, Tribological
Celcon M90SW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear against the same mating surface is important. This grade may be preferre..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® M90UV POM, UV Resistant
Celcon« M90UV is an acetal copolymer developed as a natural UV light stabilized standard flow grade for overall performance in most molding applications. It has been formulated as a natural acetal ..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celstran® POM-GF25-04 AF3001 POM, 25% Glass Reinforced
Material code according to ISO 1043-1: POMInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 9021 XAP2 LS POM, UV Resistant
POM copolymerInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® LU-02XAP® POM, UV Resistant
Hostaform« acetal copolymer grade LU-02 XAP« is UV stabilized material displaying a reduced gloss over standard UV acetal grades similar to LU-02. However, Hostaform« LU-02XAP« has lower volati..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® M90XAP® POM, Unfilled
Hostaform« acetal copolymer grade M90 XAP« is a low emission version, medium viscosity polymer providing optimum performance in general purpose injection molding primarily for the interior automo..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified
Preliminary Data SheetInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celstran® POM-GF35-04 AF3001 POM, 35% Glass Reinforced
Material code according to ISO 1043-1: POMInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® S 9363 POM, Impact Modified
Hostaform« acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform« S 9363 provides good impact strength while improving modulus and weld line strength o..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® S 9243 XAP2 ™ POM, Impact Modified
POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® M450 POM  (Unverified Data**)
Celcon® acetal copolymer grade M450 is an extremely low viscosity grade for optimal cycle performance in very thin walls or long, narrow flow paths in injection molding.Very high flow, fast cycling..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 13021 RM POM, Tribological  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with moderate flow, with improved friction propertiesInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 9021 GV3/20 POM, 20% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 20 % glass spheresInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® LM90 POM, Specialty  (Unverified Data**)
Hostaform® LM90 is a nominal 9 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform® LM90 can be laser marked with barcodes, identif..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® S 9362 POM, Impact Modified  (Unverified Data**)
Hostaform® acetal copolymer grade S 9362 is an impact modified grade for applications requiring improved impact. Hostaform® S 9362 provides good impact strength while improving modulus and weld ..
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 13021 RM POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 9021 GV1/20 POM, 20% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 9021 GV3/20 POM, 20% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® MT® SlideX™ 2404 POM, Medical Technology
POM copolymerInformation provided by Celanese
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® MC270-HM POM, Mineral Reinforced
Celcon« MC270-HM is a high modulus, mineral coupled acetal copolymer. It utilizes a higher additive level to provide significant improvement in product stiffness and mold shrinkage and better warp..