Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 55.2 - 103 MPa | 8000 - 15000 psi | |
RheTech Products FT4802-692UV Thermoplastic Polyolefin, UV Stabilized, RS8 Grey Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 55.2 - 103 MPa | 8000 - 15000 psi | |
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 55.2 - 103 MPa | 8000 - 15000 psi | |
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 55.2 - 103 MPa | 8000 - 15000 psi | |
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 55.2 - 103 MPa | 8000 - 15000 psi | |
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 55.2 - 82.7 MPa | 8000 - 12000 psi | |
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 55.2 - 82.7 MPa | 8000 - 12000 psi | Average value: 68.9 MPa Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |