Processing Properties Metric English Comments
Processing Temperature 350 - 410 °C
662 - 770 °F
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer  (discontinued **)
Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420
Processing Temperature 371 - 410 °C
700 - 770 °F
Average value: 384 °C Grade Count:3
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Processing Temperature 385 - 410 °C
725 - 770 °F
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:..