Category Polymer , Thermoplastic , Fluoropolymer , PFA , Polyperfluoroalkoxyethylene, Molded/Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420
Physical Properties Metric English Comments
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
Water Absorption <= 0.050 %
<= 0.050 %
Linear Mold Shrinkage 0.040 - 0.060 cm/cm
0.040 - 0.060 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength, Ultimate 22.0 - 28.0 MPa
3190 - 4060 psi
Elongation at Break >= 300 %
>= 300 %
>= 400 %

@Temperature 250 °C
>= 400 %

@Temperature 482 °F
Flexural Modulus 0.600 - 0.650 GPa
87.0 - 94.3 ksi
Izod Impact, Notched NB
NB
ASTM D256
Izod Impact, Unnotched NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
(Notch not specified)
Charpy Impact Unnotched NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
Notch not specified
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C

@Temperature 20.0 °C
66.7 µin/in-°F

@Temperature 68.0 °F
140 µm/m-°C

@Temperature 100 °C
77.8 µin/in-°F

@Temperature 212 °F
250 µm/m-°C

@Temperature 200 °C
139 µin/in-°F

@Temperature 392 °F
Melting Point >= 300 °C
>= 572 °F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
Oxygen Index >= 95 %
>= 95 %
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+17 ohm-cm

@Temperature 23.0 - 150 °C
>= 1.00e+17 ohm-cm

@Temperature 73.4 - 302 °F
Surface Resistance >= 1.00e+17 ohm
>= 1.00e+17 ohm
Dielectric Constant 2.1

@Frequency 50 Hz
2.1

@Frequency 50 Hz
Dielectric Strength 34.0 kV/mm

@Thickness 1.00 mm
864 kV/in

@Thickness 0.0394 in
Dissipation Factor 0.00030 - 0.0080

@Frequency 50 Hz,
Temperature 23.0 - 150 °C
0.00030 - 0.0080

@Frequency 50 Hz,
Temperature 73.4 - 302 °F
Processing Properties Metric English Comments
Processing Temperature 350 - 410 °C
662 - 770 °F