Processing Properties Metric English Comments
Processing Temperature 350 - 400 °C
662 - 752 °F
PolyChem Alloy PolyFoam HDC5
PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph..
Processing Temperature 350 - 410 °C
662 - 770 °F
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer  (discontinued **)
Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber
Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE
Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-7725 VP Polyether sulfone, with glass fiber, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-7939/GY Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-8194 Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and ..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-8326 Polyether sulfone, with carbon fiber, PTFE, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR Polyether sulfone, with glass fiber, easy flowing, demolding aid
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR/BK Polyether sulfone, with glass fiber, easy flowing, demolding aid
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100/GF/30/NAT Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-7337/WT Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-7721/WT9016 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-7890 Polyether sulfone, with carbon fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-8049 Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
mass temp
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Processing Temperature 350 °C
662 °F
Shinil Chemical SHINCON PEI-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..