Polymer Property : Processing Temperature = 700 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 371 °C
700 °F
Plasma Coatings 200 Surface Material
Information provided by Plasma Coatings
Processing Temperature 371 °C
700 °F
Plasma Coatings 15000 Surface Material
Information provided by Plasma Coatings
Processing Temperature 371 - 410 °C
700 - 770 °F
Average value: 384 °C Grade Count:3
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..