Material Notes:
Unfilled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.015 %
0.015 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 68.9 MPa
10000 psi
ASTM D638
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 125 %
125 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 2.38 GPa
345 ksi
ASTM D638
Flexural Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Compressive Strength 86.2 MPa
12500 psi
ASTM D695
Izod Impact, Notched 6.94 J/cm

@Temperature 23.0 °C
13.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
265 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Processing Temperature 271 °C
520 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved