S&E Specialty Polymers TufFlex™ GA-509-75 TPE Compound

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer S&E Specialty Polymers
Trade Name TufFlex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFlex™ GA-509-75 TPE Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A UL listed, sunlight resistant, 75°C rated, UL1277 power limited and control cable jacketing compound for CMX, CL2 and CL3 applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75.0

@Time 15.0 sec
75.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 11.8 MPa
1710 psi
ASTM D412
11.8 MPa

@Temperature 100 °C,
Time 864000 sec
1710 psi

@Temperature 212 °F,
Time 240 hour
Aged
Elongation at Break 385 %
385 %
ASTM D412
327.25 %

@Treatment Temp. 100 °C,
Time 864000 sec
327.25 %

@Treatment Temp. 212 °F,
Time 240 hour
Aged
100% Modulus 0.00793 GPa
1.15 ksi
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 28.0 %
28.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 171 - 182 °C
340 - 360 °F
Suggested Stock