Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Advanced Polymer Alloys DuraGrip™ DGR 6040 NCHT Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer APA - Advanced Polymer Alloys
Trade Name DuraGrip™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys DuraGrip™ DGR 6040 NCHT Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraGrip® DGR 6040NCHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with improved surface tack that produces superior grip qualities. DGR 6040NCHT, will bond to olefinics, and is easily colored. DuraGrip® DGR 6040NCHT is not hygroscopic and under normal conditions does not require drying.Information provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
ASTM D471; ISO 2781
Viscosity 127000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
127000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Time of 5 seconds; ASTM D2240; ISO 48
Tensile Strength, Ultimate 4.96 MPa
720 psi
ASTM D412; ISO 37
Elongation at Break 751 %
751 %
ASTM D412; ISO 37
100% Modulus 0.00121 GPa
0.175 ksi
ASTM D412; ISO 37
Processing Properties Metric English Comments
Processing Temperature 216 °C
420 °F