Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific)
Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5..
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC
LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific)
LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi..
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX04490 PC
LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® EH7025AG PBT+PET
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC (Asia Pacific)
LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 (Asia Pacific)
LNP Thermocomp RF008 is a compound based on PA66 resin containing glass fiber. It is used in many applications requiring high strength over weight performance. Also known as Thermocomp RF-1008
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP QFL17RS PA 6/10
LNP LUBRICOMP* QFL17RS is a compound based on Nylon 6/10 resin containing 35% Glass Fiber, 5% PTFE. Added features of this material include: Easy Release, Heat Stabilized, Wear Resistant.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT
LNP* STAT-LOY* WF306C is a compound based on PBT resin containing 30% Glass Fiber. Added features of this material include: Antistat, Clean Compound System.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific)
LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC
LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific)
LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC
LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC (Asia Pacific)
LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp GL004 PSU
LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re..
CTE, linear, Transverse to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific)
LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.