Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 47.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG94 ABS
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG94 ABS
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG94U ABS
High flow, UV stabilized ABS molding grade
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications.
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications.
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 500ECR PC
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® 500ECR PC
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 500ECR PC (Asia Pacific)
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® 500ECR PC (Asia Pacific)
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East)
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East)
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 505R PC
Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm...
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 505R PC (Asia Pacific)
Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm...
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 505R PC (Europe-Africa-Middle East)
Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm...
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature 25.6 - 93.3 °C
47.0 µin/in-°F

@Temperature 78.0 - 200 °F
Diameter
Saint-Gobain Rulon® W2 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific)
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific)
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA
Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W..
CTE, linear, Transverse to Flow 84.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA
Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W..