Thermal Properties Metric English Comments
Thermal Conductivity 0.600 - 0.700 W/m-K

@Temperature 600 °C
4.16 - 4.86 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 127 S Dense Refractory Castable
Description: Curon 127 S castable is characterized by a very high strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks: These value..
Thermal Conductivity 0.500 - 0.700 W/m-K

@Temperature 200 °C
3.47 - 4.86 BTU-in/hr-ft²-°F

@Temperature 392 °F
Gouda Vuurvast FI 35-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.500 - 0.700 W/m-K

@Temperature 200 °C
3.47 - 4.86 BTU-in/hr-ft²-°F

@Temperature 392 °F
Gouda Vuurvast FI 45-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.500 - 0.700 W/m-K

@Temperature 1000 °C
3.47 - 4.86 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast FI 65-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.600 - 0.700 W/m-K

@Temperature 600 °C
4.16 - 4.86 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 145 C Dense Refractory Castable
Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information ..
Thermal Conductivity 0.600 - 0.700 W/m-K

@Temperature 600 °C
4.16 - 4.86 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 145 Dense Refractory Castable
Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products...