Gouda Vuurvast CURON 145 Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 145 Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.15 - 2.25 g/cc
0.0777 - 0.0813 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1300 °C
5080 - 6530 psi

@Temperature 2370 °F
Cold Crushing Strength
50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 100 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.600 - 0.700 W/m-K

@Temperature 600 °C
4.16 - 4.86 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.670 - 0.770 W/m-K

@Temperature 1300 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1450 °C
2640 °F
Shrinkage -0.300 - 0.300 %

@Temperature 1300 °C
-0.300 - 0.300 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 45 %
45 %
Fe2O3 <= 2.0 %
<= 2.0 %
SiO2 44 %
44 %
Descriptive Properties Value Comments
ASTM Classification C
Material Consumption per 1 m3 2150 kg
Mixing Water 10-12 liters
per 100 kgs dry material