Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.600 - 0.700 W/m-K @Temperature 600 °C |
4.16 - 4.86 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 127 S Dense Refractory Castable Description: Curon 127 S castable is characterized by a very high strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks: These value.. |
|||
Thermal Conductivity | 0.500 - 0.700 W/m-K @Temperature 200 °C |
3.47 - 4.86 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast FI 35-15 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.500 - 0.700 W/m-K @Temperature 200 °C |
3.47 - 4.86 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast FI 45-15 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.500 - 0.700 W/m-K @Temperature 1000 °C |
3.47 - 4.86 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast FI 65-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.600 - 0.700 W/m-K @Temperature 600 °C |
4.16 - 4.86 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 145 C Dense Refractory Castable Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information .. |
|||
Thermal Conductivity | 0.600 - 0.700 W/m-K @Temperature 600 °C |
4.16 - 4.86 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 145 Dense Refractory Castable Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products... |