Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.500 - 0.600 W/m-K @Temperature 100 °C |
3.47 - 4.16 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 145 F Sp Dense Refractory Castable Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variet.. |
|||
Thermal Conductivity | 0.500 - 0.700 W/m-K @Temperature 200 °C |
3.47 - 4.86 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast FI 35-15 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.500 - 0.700 W/m-K @Temperature 200 °C |
3.47 - 4.86 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast FI 45-15 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.500 - 0.700 W/m-K @Temperature 1000 °C |
3.47 - 4.86 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast FI 65-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |