Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.670 - 0.770 W/m-K @Temperature 1000 °C |
4.65 - 5.34 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast CURON 150 AC Dense Refractory Castable Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.670 - 0.770 W/m-K @Temperature 1300 °C |
4.65 - 5.34 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 150 HS Dense Refractory Castable Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.670 - 0.770 W/m-K @Temperature 600 °C |
4.65 - 5.34 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 160 HC Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s.. |
|||
Thermal Conductivity | 0.670 - 0.770 W/m-K @Temperature 600 °C |
4.65 - 5.34 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 160 HF Dense Refractory Castable Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the .. |
|||
Thermal Conductivity | 0.670 - 0.770 W/m-K @Temperature 1300 °C |
4.65 - 5.34 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 145 C Dense Refractory Castable Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information .. |
|||
Thermal Conductivity | 0.670 - 0.770 W/m-K @Temperature 1300 °C |
4.65 - 5.34 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 145 Dense Refractory Castable Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products... |
|||
Thermal Conductivity | 0.670 - 0.770 W/m-K @Temperature 100 °C |
4.65 - 5.34 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 150 GM Dense Refractory Castable Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro.. |
|||
Thermal Conductivity | 0.670 - 0.770 W/m-K @Temperature 600 °C |
4.65 - 5.34 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 160 HS Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc.. |
|||
Thermal Conductivity | 0.670 - 0.770 W/m-K @Temperature 600 °C |
4.65 - 5.34 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva.. |