Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.70 - 1.80 g/cc
0.0614 - 0.0650 lb/in³
After drying at 110°C
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 20.0 - 30.0 MPa

@Temperature 100 °C
2900 - 4350 psi

@Temperature 212 °F
Cold Crushing Strength
20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.370 - 0.470 W/m-K

@Temperature 100 °C
2.57 - 3.26 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.420 - 0.520 W/m-K

@Temperature 600 °C
2.91 - 3.61 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.450 - 0.550 W/m-K

@Temperature 1000 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
Shrinkage -0.300 - 0.300 %

@Temperature 1000 °C
-0.300 - 0.300 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 32 %
32 %
SiO2 48 %
48 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 1700 kg
Mixing Water 13-16 liters
per 100 kgs dry material