Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 2.50 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.360 W/m-K

@Temperature 538 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Pyrotek Pyrocast 80 Lightweight Castable Refractory
Pyrocast 80 is a lightweight, low cement, fused silica castable designed for moderate flow molten aluminum contact applications. Pyrocast 80 offers low thermal conductivity, excellent resistance to..
Thermal Conductivity 0.360 W/m-K

@Temperature 100 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company
Thermal Conductivity 0.360 - 0.460 W/m-K

@Temperature 100 °C
2.50 - 3.19 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 145 Refractory Insulating Castable
Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also avail..
Thermal Conductivity 0.360 - 0.460 W/m-K

@Temperature 100 °C
2.50 - 3.19 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 155 Refractory Insulating Castable
Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available i..
Thermal Conductivity 0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
4 pcf
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thermal Conductivity 0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
4 pcf
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Thermal Conductivity 0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
4 pcf
Thermal Ceramics Cerachrome Blanket
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg..
Thermal Conductivity 0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
4 pcf
Thermal Ceramics Kaowool S Blanket
Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F ..
Thermal Conductivity 0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C201
Thermal Ceramics TC-26 HS High Temperature Insulating Firebrick
The bond developed is a ceramic bond that is formed by high temperature firing. This produces bricks that are very stable and strong at temperatures higher than 2600°F (1427°C). Features:High temp..
Thermal Conductivity 0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-25 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-26 HS Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.360 W/m-K

@Temperature 1093 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials C-22 Z Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.360 W/m-K

@Temperature 600 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C182
BNZ Materials Color CA Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.360 W/m-K

@Temperature 982 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1800 °F
3M 615+ Fire Barrier Duct Wrap
3M Fire Barrier Duct Wrap 615+ is a flexible fire-resistant wrap consisting of an inorganic fiber blanket encapsulated with a scrim-reinforced foil. The product is 1-1/2 in. thick, 6pcf density. It ..
Thermal Conductivity 0.360 W/m-K

@Temperature 100 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC085 Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of PPS and other proprietary fillers blended with PTFE.Information provided by Dyneon, A 3M Company
Copyright © lookpolymers.com All Rights Reserved