Thermal Properties Metric English Comments
Thermal Conductivity 0.360 W/m-K

@Temperature 538 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Pyrotek Pyrocast 80 Lightweight Castable Refractory
Pyrocast 80 is a lightweight, low cement, fused silica castable designed for moderate flow molten aluminum contact applications. Pyrocast 80 offers low thermal conductivity, excellent resistance to..
Thermal Conductivity 0.360 W/m-K

@Temperature 100 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company
Thermal Conductivity 0.360 - 0.460 W/m-K

@Temperature 100 °C
2.50 - 3.19 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 145 Refractory Insulating Castable
Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also avail..
Thermal Conductivity 0.360 - 0.460 W/m-K

@Temperature 100 °C
2.50 - 3.19 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 155 Refractory Insulating Castable
Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available i..
Thermal Conductivity 0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-25 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-26 HS Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.360 W/m-K

@Temperature 1093 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials C-22 Z Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.360 W/m-K

@Temperature 600 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C182
BNZ Materials Color CA Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.360 W/m-K

@Temperature 982 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1800 °F
3M 615+ Fire Barrier Duct Wrap
3M Fire Barrier Duct Wrap 615+ is a flexible fire-resistant wrap consisting of an inorganic fiber blanket encapsulated with a scrim-reinforced foil. The product is 1-1/2 in. thick, 6pcf density. It ..
Thermal Conductivity 0.360 W/m-K

@Temperature 100 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530