3M 615+ Fire Barrier Duct Wrap

Category Other Engineering Material
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 615+ Fire Barrier Duct Wrap.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Fire Barrier Duct Wrap 615+ is a flexible fire-resistant wrap consisting of an inorganic fiber blanket encapsulated with a scrim-reinforced foil. The product is 1-1/2 in. thick, 6pcf density. It is used to fire rate commercial kitchen grease ducts as well as ventilation ducts. It is proven alternative to 1- or 2-hour fire-resistant rated shaft enclosures for grease ducts (ICC-ES ESR-1255). With its excellent insulating capabilities, low weight and thin profile, it is an ideal choice for a duct enclosure system. This non-asbestos wrap installs easily due to its high flexibility and strength.Information provided by 3M
Thermal Properties Metric English Comments
Thermal Conductivity 0.0900 W/m-K

@Temperature 260 °C
0.625 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.170 W/m-K

@Temperature 537 °C
1.18 BTU-in/hr-ft²-°F

@Temperature 999 °F
0.280 W/m-K

@Temperature 815 °C
1.94 BTU-in/hr-ft²-°F

@Temperature 1500 °F
0.360 W/m-K

@Temperature 982 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1800 °F
0.430 W/m-K

@Temperature 1093 °C
2.98 BTU-in/hr-ft²-°F

@Temperature 1999 °F
Shrinkage 1.20 %

@Temperature 1000 °C,
Time 86400 sec
1.20 %

@Temperature 1830 °F,
Time 24.0 hour
Linear
Descriptive Properties Value Comments
Appearance Aluminum with Black Text
Scrim color
White
Blanket color
Copyright © lookpolymers.com All Rights Reserved