Thermal Properties Metric English Comments
Thermal Conductivity 0.100 W/m-K

@Temperature 316 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 601 °F
Pyrotek I-14 Insulating Board
Pyrotek's I-14 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-14 also contains no RDF's.A..
Thermal Conductivity 0.100 W/m-K

@Temperature 425 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 797 °F
Pyrotek M-14 Compressible/Insulating Boards
ApplicationsSiphon gaskets Trough and ladle linings Tundishes Mill board substitute AdvantagesResistant to chemical attack Excellent thermal shock resistance Slightly flexible Moderately compressibl..
Thermal Conductivity 0.100 W/m-K

@Temperature 260 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 500 °F
Pyrotek Pyrocast L-40 Insulating Refractory
Pyrocast L-40 is a fiber free refractory moldable designed for use in contact with molten aluminum. L-40 has excellent workability for use as an insulating lining or patching material.Recommended C..
Thermal Conductivity 0.100 - 0.160 W/m-K

@Temperature 600 °C
0.694 - 1.11 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable
Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning ..
Thermal Conductivity 0.100 - 0.180 W/m-K

@Temperature 100 °C
0.694 - 1.25 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 1.0.6. Mix Refractory Insulating Castable
Description: This castable is composed of a high quality alumina cement and vermiculite and is applied as a backlining. Special additives are responsible for the low shrinkage. This castable can be ..
Thermal Conductivity 0.100 W/m-K

@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Thermal Conductivity 0.100 W/m-K

@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Thermal Conductivity 0.100 W/m-K

@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Thermal Conductivity 0.100 W/m-K

@Temperature 400 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 752 °F
Zircar Ceramics AXL Alumina-Silica Insulation
ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a..
Thermal Conductivity 0.100 W/m-K

@Temperature 400 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C177-76
Zircar Ceramics Uniform A2 Alumina-Silica Insulation
ZIRCAR Alumina-Silica Insulation Type "UNIFORM A"  is a family of refractory ceramic fiber based insulations with exceptional machineability and strength. They are made of specially prepared alumi..
Thermal Conductivity 0.100 W/m-K

@Temperature 400 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 752 °F
parallel to thickness
Zircar Ceramics Z-MAG/2300 Soluble Fiber Insulation
ZIRCAR NON-RCF Insulation Type Z-MAG/2300 is a rigid combination of soluble NON-RCF silica magnesia glass fibers and inorganic binder. It is suitable for use as a substitute for insulation containin..
Thermal Conductivity 0.100 W/m-K

@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 1110 °F
parallel to thickness
Zircar Refractory Composites ZIRCAL-18 Refractory Board
Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value m..
Thermal Conductivity 0.100 W/m-K

@Temperature 538 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Zircar Ceramics APA-1 Alumina Paper
ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-1 is a strong, flexible material with fibers held together with organic binder that is available in roll or sheet..
Thermal Conductivity 0.100 W/m-K

@Temperature 538 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Zircar Ceramics APA-2 Alumina Paper
ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-2 is a flexible un-bonded sheet that contains no organic binder. Applications include thermal insulation in low ..
Thermal Conductivity 0.100 W/m-K

@Temperature 500 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 932 °F
parallel to thickness; ASTM C177
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE
ZIRCAR Alumina-Silica Insulating Blanket Type RS-B Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped ..
Thermal Conductivity 0.100 W/m-K

@Temperature 175 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 347 °F
ASTM D1674
DuPont™ Nomex® Type 993, 160 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Thermal Conductivity 0.100 W/m-K

@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C182
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.
Thermal Conductivity 0.100 W/m-K

@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C182
BNZ Materials Zelieblok 2000S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.
Thermal Conductivity 0.100 W/m-K

@Temperature 316 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 601 °F
3M Interam™ E-5A-4 Endothermic Mat
When properly installed, 3M Interam Endothermic Mat E-5A-4 provides a uniform covering that, when exposed to high temperatures, releases chemically-bound water to cool the outer surfaces of the wrap..