Material Notes:
ApplicationsSiphon gaskets Trough and ladle linings Tundishes Mill board substitute AdvantagesResistant to chemical attack Excellent thermal shock resistance Slightly flexible Moderately compressible Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.352 g/cc
0.0127 lb/in³
Loss On Ignition 6.0 %
6.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000790 GPa

@Treatment Temp. 815 °C
0.115 ksi

@Treatment Temp. 1500 °F
Compressive Strength 0.280 MPa
40.6 psi
to 10% deformation
Thermal Properties Metric English Comments
Thermal Conductivity 0.0900 W/m-K

@Temperature 240 °C
0.625 BTU-in/hr-ft²-°F

@Temperature 464 °F
0.100 W/m-K

@Temperature 425 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 797 °F
0.160 W/m-K

@Temperature 870 °C
1.11 BTU-in/hr-ft²-°F

@Temperature 1600 °F
Maximum Service Temperature, Air 1620 °C
2950 °F
Continuous
Component Elements Properties Metric English Comments
Al2O3 42 %
42 %
SiO2 46 %
46 %
Users viewing this material also viewed the following: