Material Notes:
ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-1 is a strong, flexible material with fibers held together with organic binder that is available in roll or sheet form. Applications include thermal insulation in low mass furnaces and thermal process systems operating to 1650°C (3002°F) high temperature gaskets and seals, separator in multifoil vacuum furnace insulation systems, expansion joint insulation, backup thermal insulation in molten metal troughs, furnaces and thermal process systems operating to high temperatures, and parting agent and barrier layer in brazing, heat-treating and metal forming processes.Information provided by Zircar Ceramics.
Physical Properties Metric English Comments
Density 0.150 g/cc

@Thickness 1.02 mm
0.00542 lb/in³

@Thickness 0.0400 in
0.150 g/cc

@Thickness 3.05 mm
0.00542 lb/in³

@Thickness 0.120 in
0.200 g/cc

@Thickness 0.508 mm
0.00723 lb/in³

@Thickness 0.0200 in
Mechanical Properties Metric English Comments
Tear Strength 0.456 kN/m
2.60 pli
Parallel to Thickness, width
0.202 kN/m

@Thickness 0.508 mm
1.15 pli

@Thickness 0.0200 in
0.263 kN/m

@Thickness 1.02 mm
1.50 pli

@Thickness 0.0400 in
0.806 kN/m

@Thickness 3.05 mm
4.60 pli

@Thickness 0.120 in
Thermal Properties Metric English Comments
Thermal Conductivity 0.100 W/m-K

@Temperature 538 °C
0.694 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.260 W/m-K

@Temperature 1370 °C
1.80 BTU-in/hr-ft²-°F

@Temperature 2500 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Component Elements Properties Metric English Comments
Al2O3 79 %

@Thickness 1.02 - 3.05 mm
79 %

@Thickness 0.0400 - 0.120 in
85 %

@Thickness 0.508 mm
85 %

@Thickness 0.0200 in
Other 2.0 %

@Thickness 0.508 mm
2.0 %

@Thickness 0.0200 in
Other Oxides
<= 4.0 %

@Thickness 1.02 - 3.05 mm
<= 4.0 %

@Thickness 0.0400 - 0.120 in
Other Oxides
6.0 %

@Thickness 0.508 mm
6.0 %

@Thickness 0.0200 in
Organic
8.0 %

@Thickness 1.02 - 3.05 mm
8.0 %

@Thickness 0.0400 - 0.120 in
Organic
SiO2 7.0 %

@Thickness 0.508 mm
7.0 %

@Thickness 0.0200 in
9.0 %

@Thickness 1.02 - 3.05 mm
9.0 %

@Thickness 0.0400 - 0.120 in
Descriptive Properties Value Comments
Color White
Form Flexible
Type of Binder Organic
Weight 100 g/m2
0.02" Thickness
150 g/m2
0.04" Thickness
450 g/m2
0.12" Thickness