Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.590 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.590 W/m-K

@Temperature 650 °C
4.09 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Pyrotek Dry Cathode Barrier Material
In the presence of cryolite, Dri-Barrier Mix is designed to form a viscous layer on its surface which prevents further penetration. The freezing isotherm sustained in Dri-Barrier Mix decreases the ..
Thermal Conductivity 0.590 W/m-K

@Temperature 400 °C
4.09 BTU-in/hr-ft²-°F

@Temperature 752 °F
Pyrotek Pyrocast AR Castable Refractory
Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro..
Thermal Conductivity 0.590 W/m-K

@Temperature 400 °C
4.09 BTU-in/hr-ft²-°F

@Temperature 752 °F
Pyrotek Pyrocast AR FINE Castable Refractory
Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting..
Thermal Conductivity 0.590 - 0.690 W/m-K

@Temperature 100 °C
4.09 - 4.79 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable
Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord..
Thermal Conductivity 0.590 W/m-K

@Temperature 538 °C
4.09 BTU-in/hr-ft²-°F

@Temperature 1000 °F
ASTM C182
BNZ Materials BNZ-32 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..