Polymer Property : Thermal Conductivity = 0.690 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.590 - 0.690 W/m-K

@Temperature 100 °C
4.09 - 4.79 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable
Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord..
Thermal Conductivity 0.490 - 0.690 W/m-K

@Temperature 200 °C
3.40 - 4.79 BTU-in/hr-ft²-°F

@Temperature 392 °F
Gouda Vuurvast FI 65-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.490 - 0.690 W/m-K

@Temperature 600 °C
3.40 - 4.79 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 65-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.