Category Ceramic , Oxide , Silicon Oxide
Manufacturer Pyrotek, Inc.
Trade Name Pyrocast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyrocast AR Castable Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyrocast AR are heat-treated to ensure free and combined water are removed. Pyrocast AR floats in aluminum, minimizing the potential for refractory inclusions.ApplicationsHot-top table sections Transfer & stub troughs Launder linings Filter boxes Sheet ingot spouts Control pins Furnace tubes AdvantagesDimensionally stable Thermal shock resistant Easily cleaned Extremely durable Smooth cast surface Preheating unnecessary Non-wetting Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.86 - 1.89 g/cc
0.0672 - 0.0683 lb/in³
Open Porosity 20 - 24 %
20 - 24 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00690 GPa

@Treatment Temp. 649 °C
1.00 ksi

@Treatment Temp. 1200 °F
0.0103 GPa

@Treatment Temp. 815 °C
1.49 ksi

@Treatment Temp. 1500 °F
Flexural Strength 9.00 MPa
1310 psi
Compressive Strength 41.4 MPa
6000 psi
cured at 649°C
Thermal Properties Metric English Comments
CTE, linear 0.810 µm/m-°C

@Temperature 649 °C
0.450 µin/in-°F

@Temperature 1200 °F
Thermal Conductivity 0.590 W/m-K

@Temperature 400 °C
4.09 BTU-in/hr-ft²-°F

@Temperature 752 °F
0.710 W/m-K

@Temperature 550 °C
4.93 BTU-in/hr-ft²-°F

@Temperature 1020 °F
0.820 W/m-K

@Temperature 700 °C
5.69 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Maximum Service Temperature, Air 760 °C
1400 °F
Not recommended for use in continuous casting applications.
Shrinkage 0.200 - 0.250 %

@Treatment Temp. 725 °C
0.200 - 0.250 %

@Treatment Temp. 1340 °F
Component Elements Properties Metric English Comments
Al2O3 16 %
16 %
CaO 4.0 %
4.0 %
SiO2 80 %
80 %