Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0600 W/m-K @Temperature 93.0 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 199 °F |
|
Pyrotek I-14 Insulating Board Pyrotek's I-14 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-14 also contains no RDF's.A.. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Mid-Mountain Materials CERMEX® BK1800SW Low Biopersistence Thermal Insulation Blanket Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Mid-Mountain Materials CERMEX® BK2200SW Low Biopersistence Thermal Insulation Blanket Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 200 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 392 °F |
N<sub>2</sub>; ASTM C177 |
Mid-Mountain Materials CERMEX® PR1000-C Commercial Grade Thermal Insulation Paper Material: Non-respirable E-glass fibers Construction: Felted paper, organic binderInformation provided by Mid-Mountain Materials |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 200 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 392 °F |
Air; ASTM C114 |
Mid-Mountain Materials CERMEX® PR1000-C Commercial Grade Thermal Insulation Paper Material: Non-respirable E-glass fibers Construction: Felted paper, organic binderInformation provided by Mid-Mountain Materials |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Mid-Mountain Materials CERMEX® PR1000-P Premium Grade Thermal Insulation Paper Material: Non-respirable E-glass fibers Construction: Felted paper, organic binderInformation provided by Mid-Mountain Materials |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Mid-Mountain Materials CERMEX® PR2200SW Thermal Insulation Mat Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 200 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
8 pcf |
Thermal Ceramics Cerablanket Blanket Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave.. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
8 pcf |
Thermal Ceramics Cerachem Blanket Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe.. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
8 pcf |
Thermal Ceramics Cerachrome Blanket Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg.. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
8 pcf |
Thermal Ceramics Kaowool S Blanket Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F .. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 250 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 482 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 200 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 392 °F |
ASTM C177 |
Zircar Refractory Composites RS-C ALUMINA-SILICA MOLDABLE ZIRCAR Alumina-Silica Insulating Blanket Type RS-C Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped .. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 500 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct.. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 200 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 392 °F |
ASTM C182 |
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation Information provided by BNZ Materials Inc. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 149 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 300 °F |
|
Thermal Ceramics Kaomat Blanket Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets... |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Thermal Ceramics Kaomat SL Blanket Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets... |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
8 pcf |
Thermal Ceramics Kaowool Blanket Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of dens.. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 250 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 482 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics ZAL-15 Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 500 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |