Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.0600 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0600 W/m-K

@Temperature 93.0 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 199 °F
Pyrotek I-14 Insulating Board
Pyrotek's I-14 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-14 also contains no RDF's.A..
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
Mid-Mountain Materials CERMEX® BK1800SW Low Biopersistence Thermal Insulation Blanket
Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
Mid-Mountain Materials CERMEX® BK2200SW Low Biopersistence Thermal Insulation Blanket
Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.0600 W/m-K

@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 392 °F
N<sub>2</sub>; ASTM C177
Mid-Mountain Materials CERMEX® PR1000-C Commercial Grade Thermal Insulation Paper
Material: Non-respirable E-glass fibers Construction: Felted paper, organic binderInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.0600 W/m-K

@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 392 °F
Air; ASTM C114
Mid-Mountain Materials CERMEX® PR1000-C Commercial Grade Thermal Insulation Paper
Material: Non-respirable E-glass fibers Construction: Felted paper, organic binderInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
Mid-Mountain Materials CERMEX® PR1000-P Premium Grade Thermal Insulation Paper
Material: Non-respirable E-glass fibers Construction: Felted paper, organic binderInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper
Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
Mid-Mountain Materials CERMEX® PR2200SW Thermal Insulation Mat
Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.0600 W/m-K

@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf
Thermal Ceramics Cerachrome Blanket
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg..
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf
Thermal Ceramics Kaowool S Blanket
Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F ..
Thermal Conductivity 0.0600 W/m-K

@Temperature 250 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 482 °F
parallel to thickness; ASTM C177-76
Zircar Ceramics ZAL-15AA Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Thermal Conductivity 0.0600 W/m-K

@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 392 °F
ASTM C177
Zircar Refractory Composites RS-C ALUMINA-SILICA MOLDABLE
ZIRCAR Alumina-Silica Insulating Blanket Type RS-C Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped ..
Thermal Conductivity 0.0600 W/m-K

@Temperature 500 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 932 °F
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper
ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct..
Thermal Conductivity 0.0600 W/m-K

@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 392 °F
ASTM C182
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.
Thermal Conductivity 0.0600 W/m-K

@Temperature 149 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 300 °F
Thermal Ceramics Kaomat Blanket
Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets...
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
Thermal Ceramics Kaomat SL Blanket
Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets...
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf
Thermal Ceramics Kaowool Blanket
Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of dens..
Thermal Conductivity 0.0600 W/m-K

@Temperature 250 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 482 °F
parallel to thickness; ASTM C177-76
Zircar Ceramics ZAL-15 Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Thermal Conductivity 0.0600 W/m-K

@Temperature 500 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 932 °F
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper
ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c..