Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 154 °C

@Load 1.00 kg
309 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Vicat Softening Point 154 °C

@Load 1.02 kg
309 °F

@Load 2.25 lb
ISO 306
Borealis BC612WG Polypropylene Copolymer
BC612WG is a polypropylene copolymer intended for injection molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical..
Vicat Softening Point 154 °C

@Load 1.02 kg
309 °F

@Load 2.25 lb
ISO 306
Borealis HB601WG Polypropylene Homopolymer
HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent ..
Vicat Softening Point 154 °C

@Load 1.02 kg
309 °F

@Load 2.25 lb
ISO 306
Borealis PS65T20 Polypropylene Compound, Mineral Filled
PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic..
Vicat Softening Point 154 °C

@Load 1.02 kg
309 °F

@Load 2.25 lb
ISO 306
Borealis MS64T20 Polypropylene Compound, Mineral Filled
MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p..