Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 154 °C @Load 1.00 kg |
309 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Vicat Softening Point | 154 °C @Load 1.02 kg |
309 °F @Load 2.25 lb |
ISO 306 |
Borealis BC612WG Polypropylene Copolymer BC612WG is a polypropylene copolymer intended for injection molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical.. |
|||
Vicat Softening Point | 154 °C @Load 1.02 kg |
309 °F @Load 2.25 lb |
ISO 306 |
Borealis HB601WG Polypropylene Homopolymer HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent .. |
|||
Vicat Softening Point | 154 °C @Load 1.02 kg |
309 °F @Load 2.25 lb |
ISO 306 |
Borealis PS65T20 Polypropylene Compound, Mineral Filled PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic.. |
|||
Vicat Softening Point | 154 °C @Load 1.02 kg |
309 °F @Load 2.25 lb |
ISO 306 |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |