Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 71.1 °C | 160 °F | Long Term |
Quadrant EPP Proteus® LDPE - Low Density Polyethylene (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Alcoa KAMA 3400 Super High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | Upper limit of working range |
Heatbath/Park High Speed Vacuum Quench Oil Faster quench speed than VQO above, but otherwise very similar. Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | Upper limit of working range |
Heatbath/Park Vacuum Quench Oil For use in quenching in integral vacuum furnaces. Offers excellent quenching rate and thermal stability, good viscosity, and low volatility.Information provided by Heatbath Corporation - Park Metal.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Saint-Gobain Norton® V730 Pressure Sensitive Adhesive Sealant Foam Description: Closed cell polyvinyl chloride foam sealant with pressure-sensitive adhesive on one side. The high-tack positioning adhesive grips tight on initial contact and keeps foam in place durin.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Saint-Gobain Norton® V740 Multipurpose Pressure Sensitive Adhesive Sealant Foam Description: Medium Density, Multipurpose Foam: Norseal V740 is a closed-cell polyvinyl chloride foam sealant with pressure-sensitive adhesive on one side designed to provide an economical solution .. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Saint-Gobain Norton® V760 High Density Vibration Description: Seals and Dampens Vibration: Norseal® V760 is a closed-cell PVC foam sealant with a pressure-sensitive adhesive on one side. Its high-density structure and multitude of tiny cells ac.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Saint-Gobain Norton® V780 Medium-Density Pressure Sensitive Adhesive Sealant Foam Description: Improved Performance: Norseal® V780 medium density foam sealant combines a closed cell foam substrate with a one-sided pressure-sensitive adhesive. Norseal has been specially formula.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Saint-Gobain Norton® Log Home Foam® V790 Description: Provides Positive Seal in Log Home Joints: Norseal® Log Home Foam® V790 is a medium-density foam specifically developed for log home gasketing. Under a minimum of 25 percent compr.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Saint-Gobain Norton® V770 Low-Density Pressure Sensitive Adhesive Sealant Foam Description: Low Density Foam Suitable for Sealing of Thin Gauge Metals and Plastics. Closed cell polyvinyl chloride foam sealant with pressure sensitive adhesive on one side. The tight bonding adhe.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Saint-Gobain Vendflow® E-70-V-CE Taste Barrier Tubing Formulation Description: Non-plasticized inner bore yeilds no taste: Vendflow® E-70-V-CE is specifically formulated to transfer water and beverages without imparting any "plastic" taste sometimes found in PV.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Loctite® 408 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Loctite® 4081 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Loctite® 455 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Loctite® 460 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Bostik 2107 General Purpose EVA Glue Stick Bostik 2107 General Purpose EVA Glue StickGeneral purpose for porous substrates. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Bostik 2391 Versatile, Good Hot Tack EVA Glue Stick Bostik 2391 Versatile, Good Hot Tack EVA Glue StickVersatile packaging product. Good "hot tack." |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Bostik 6390 Good Heat Resistance, General Purpose EVA Glue Stick Bostik 6390 Good Heat Resistance, General Purpose EVA Glue StickGood heat resistance. Bonds plastics, wood, porous materials. General purpose adhesion. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Alcoa KAMA 3202 Freezer Modified High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableColors availa.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Loctite® PRISM® 403 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Alcoa KAMA 4223 Impact Modified RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 50”Silicone coatingCl.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Loctite® 4031 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Maximum Service Temperature, Air | 71.1 °C | 160 °F | |
Loctite® 4601 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |