Heatbath/Park Vacuum Quench Oil

Category Fluid , Quenchant
Manufacturer Heatbath Corporation - Park Metallurgical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Heatbath/Park Vacuum Quench Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For use in quenching in integral vacuum furnaces. Offers excellent quenching rate and thermal stability, good viscosity, and low volatility.Information provided by Heatbath Corporation - Park Metallurgical.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 125 SUS
125 SUS
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.1 °C
160 °F
Upper limit of working range
Minimum Service Temperature, Air 54.4 °C
130 °F
Lower limit of working range
Flash Point 193 °C
380 °F