Bostik 2391 Versatile, Good Hot Tack EVA Glue Stick

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Bostik
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bostik 2391 Versatile, Good Hot Tack EVA Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bostik 2391 Versatile, Good Hot Tack EVA Glue StickVersatile packaging product. Good "hot tack."
Physical Properties Metric English Comments
Viscosity 1900 cP

@Temperature 177 °C
1900 cP

@Temperature 350 °F
Typical
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.1 °C
160 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Processing Properties Metric English Comments
Pot Life 0.67 min
0.67 min
Open Time
Descriptive Properties Value Comments
Color Tan