Material Notes:
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer and custom co-extrusion A/B, A/B/A, A/B/CHigh gloss cap layer availableCustom colors availableSilicone coating availableMedical grade availableFDA material available5 strategic manufacturing locationsPropertiesExceptional impact performanceExcellent for deep draw applicationsForms easilyKosher materialInformation provided by Alcoa Kama Co.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Thickness 178 - 1520 microns
7.00 - 60.0 mil
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.3 - 27.6 MPa
1500 - 4000 psi
ASTM D638
Elongation at Break 50 - 125 %
50 - 125 %
ASTM D638
Flexural Modulus 1.38 - 2.00 GPa
200 - 290 ksi
ASTM D790
Izod Impact, Notched 1.87 - 3.20 J/cm
3.50 - 6.00 ft-lb/in
ASTM D265
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.1 °C
160 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Processing Temperature 127 - 166 °C
260 - 330 °F
Thermoforming Temp
Descriptive Properties Value Comments
Resistance to Acid Good to Excellent
Resistance to Alcohols Good to Excellent
Resistance to Alkalis Excellent
Resistance to Fat, Grease, and Oil Good
Resistance to Hydrocarbon Solvents Poor
Resistance to Strong Oxidizers Poor
Yield, in²/lb/mil 26360